Laser Cutting Quality Troubleshooting - Dross, Burrs, Taper and Rough EdgesSource:Jinan Jing CNC CO.,Ltd Most laser cutting quality complaints fall into four groups: dross hanging on the lower edge, burrs, kerf taper, and a rough or striated cut face. In most cases the machine is fine and the setup has drifted. Work through the list below before calling service. Dross on the lower edge Hard dross that must be chipped off usually means insufficient energy at the bottom of the kerf or too much molten material: • Focus too high, so energy density at the exit side is low. Lower the focus in small steps and re-test; • Cutting speed too slow on thick plate, so the pool overheats and sticks; • Gas pressure too low for the thickness, so ejection is incomplete; • Nozzle worn or oversized, giving a diffuse gas jet; • On stainless with nitrogen, gas purity below specification reduces ejection. Soft, easily removed dross on thin sheet is often simply too much heat: raise speed or reduce power. Burrs and rough edges • Speed too high leaves unburnt material at the exit; • Contaminated or damaged protective lens reduces beam quality and causes striations; • Wrong assist gas for the material: nitrogen on carbon steel produces oxidation and roughness; • Nozzle alignment off center, giving an asymmetric kerf; • Plate surface rust or scale, which changes absorption unpredictably. A quick test: cut a short straight line in scrap of the same thickness and inspect both sides. Asymmetry points to alignment; consistent roughness points to optics or gas. Kerf taper • Focus too high exaggerates top-wide taper; too low exaggerates bottom-wide; • Insufficient power for thickness forces slow speeds and a wider kerf; • Poor beam quality, often from a degraded fiber or contaminated collimation optics; • Nozzle standoff too large, which spreads the jet and reduces pressure at the workpiece. Rough or striated faces Striations usually indicate an unstable melt flow. Check gas type and pressure against the thickness chart, verify the focus is on the correct side for the process, and confirm the lens is clean. On thick carbon steel with oxygen, excessive pressure causes violent oxidation and a rough face; too little pressure causes incomplete reaction. Maintenance items that prevent most of it 1. Protective lens inspection each shift; replace when coating or spatter appears; 2. Nozzle inspection for roundness and centering, replaced on a schedule rather than on failure; 3. Ceramic ring and height sensor cleanliness, since height errors mimic parameter faults; 4. Chiller temperature stability, because thermal drift changes cavity alignment; 5. Gas supply quality: dew point and purity checks, especially for nitrogen. A discipline that saves time Keep a cutting parameter log per material and thickness: power, speed, focus, gas and pressure, nozzle type, and the resulting edge quality. When a job goes wrong, the log usually reveals which variable was changed. That habit cuts troubleshooting time more than any single upgrade. JINAN JING CNC (BEJOY CNC) supports fiber laser cutting machines from 1.5kW to 30kW with parameter libraries, nozzle and lens supply, and remote diagnosis. Send the material, thickness and defect photos with your current parameters for a targeted adjustment plan. |