NEWS
让价值共享 记录企业发展脚步

Laser Welding Aluminum - Why It Is Harder Than Stainless and How to Fix It

Author:Jinan Jing CNC CO.,LtdSource:Jinan Jing CNC CO.,Ltd

Aluminum is where many new laser welding users get their first bad surprise. Settings that work on stainless do not transfer directly.

Why aluminum behaves differently

It reflects more of the laser energy, conducts heat away quickly, and has an oxide layer that melts at a much higher temperature than the base metal. Hydrogen also dissolves easily in the melt and forms porosity as it solidifies.

Start with cleaning

Remove oxide, oil and moisture from the joint. Mechanical cleaning followed by a suitable solvent is common practice. Cleaning often improves the weld more than any parameter change.

Then tune energy and shielding

Aluminum usually needs sufficient power density and well controlled travel speed. Good argon coverage is essential, and wobble can help stabilize the pool and improve gap tolerance.

Filler wire may be needed for certain alloys and joint designs. Alloy choice matters, so follow the material recommendation rather than guessing.

Quick answers

Why are my aluminum welds full of holes?

Porosity often comes from oxide, moisture, contamination or poor shielding. Clean first, then check gas coverage and parameters.

Can a handheld laser weld aluminum well?

Yes, within a suitable thickness and process window. It is less forgiving than stainless and needs better preparation.

Do I always need filler wire?

Not always, but some alloys and joints benefit from it. Test with the intended alloy before production.

Jinan Jing CNC CO.,Ltd (BEJOY CNC) can test your aluminum grade and provide starting parameters and wire recommendations.

0086-15954568354
info@jingcnc.com